Faculty of Science & Quantum Physics

Coherence Optimization in Superconducting Qubits for Room-Temperature Quantum Sensing

Authors: Prof. Marcus Vance, Dr. Maya Lin, Dr. Sarah Jenkins

Published in: Physical Review Applied & Quantum Technology, Vol. 18, 2026

DOI: 10.5555/squiz.quant.2026.0772

Executive Summary: Engineering transmon qubit Josephson junction interfaces using atomic layer deposition to mitigate dielectric surface loss and extend quantum coherence times.

Abstract

Quantum coherence times ($T_1$ and $T_2$) in superconducting transmon qubits are fundamentally constrained by high-frequency dielectric loss occurring at amorphous material interfaces and metal-substrate boundaries. Here, we present a novel surface passivation technique employing atomic layer deposition (ALD) of ultra-thin tantalum oxide ($Ta_2O_5$) capping layers on high-purity niobium-titanium nitride ($NbTiN$) superconducting resonators.


1. Physical Mechanisms of Quantum Decoherence

Superconducting circuit architectures represent a leading candidate for scalable quantum information processing and ultra-sensitive electromagnetic field detection. However, microscopic two-level systems (TLS) located within native oxide layers at the metal-air and substrate-metal interfaces cause microwave photon absorption, leading to rapid energy relaxation ($T_1$) and phase decoherence ($T_2$).

Eliminating two-level system defects requires precise atomic-scale control over surface stoichiometry, crystal orientation, and interface roughness during superconducting Josephson junction fabrication.

2. Fabrication Protocols & Material Characterization

Transmon qubit circuits were fabricated on high-resistivity silicon substrates ($\rho > 10\text{ k}\Omega\cdot\text{cm}$) using electron-beam lithography and reactive ion etching. Following native oxide removal via in-situ hydrofluoric acid etching, a $3.5\text{ nm}$ epitaxial tantalum oxide capping layer was deposited via plasma-enhanced atomic layer deposition at $250^\circ\text{C}$.

  • X-ray Photoelectron Spectroscopy (XPS): Verified total suppression of amorphous niobium pentoxide ($Nb_2O_5$) native film formation.
  • Cryogenic Measurement Setup: Qubit chips were mounted inside a dilution refrigerator at a base temperature of $12\text{ mK}$ with magnetic and infrared shielding.

3. Quantum Coherence & Sensing Performance

Microwave pulse measurements demonstrated a three-fold increase in qubit energy relaxation times, achieving average $T_1 = 312 \pm 8 \mu\text{s}$ and Ramsey dephasing times $T_2^* = 285 \pm 12 \mu\text{s}$. Applied as a quantum magnetometry sensor, the optimized transmon circuit achieved a magnetic field sensitivity of $4.2 \text{ pT}/\sqrt{\text{Hz}}$ at microwave frequencies.

4. Implications for Scalable Quantum Hardware

Surface engineering via ALD chemical passivation effectively mitigates interface dielectric loss in superconducting circuits. This chemical fabrication approach provides a scalable pathway toward fault-tolerant quantum computing gates and highly sensitive quantum sensors for biomedical magnetic resonance imaging.